Material Kinit (MPa m^0.5) J (N/mm)
PCL-BG/PUR 1.43 ± 0.04a 1.54 ± 0.10a
CaS/P 0.32 ± 0.04 0.03 ± 0.01
U-BG/PUR 0.48 ± 0.07 0.62 ± 0.10
a

p<.05, relative to either remaining material group.