Skip to main content
. 2015 Sep 10;10:5739–5750. doi: 10.2147/IJN.S82586

Figure 5.

Figure 5

Transmission electron microscopy image of the Fe3+-Mn4+-SO4/ZrO2 sample calcined at 650°C for 5 hours.