Skip to main content
. 2015 Sep 29;10:374. doi: 10.1186/s11671-015-1077-y

Fig. 4.

Fig. 4

LSV curves of a pristine Fe2O3 electrode with varying deposition time, b pristine Fe2O3 and Fe2O3-Au electrodes with different Au sputtering time, and c pristine Fe2O3 and modified Fe2O3. d Photocurrent responses of pristine Fe2O3 and modified Fe2O3 at an applied potential of 0.4 V. Electrolyte, 1 M KOH solution, illumination: a 300 W Xe lamp coupled with an AM 1.5 filter