Table 4. Ceramic surface damage index (CSDI).
Ceramic surface damage index | |||||
---|---|---|---|---|---|
0 = none | 1 = absence of glaze | 2 = presence of glaze and crack | 3 = absence of glaze and presence of crack | 4 = fracture | |
G1 - n (%) | 3 (23.07%) | 1 (7,69%) | 4 (30.76%) | 0 (0%) | 5 (38.46%) |
G2 - n (%) | 6 (54.54%) | 0 (0%) | 5 (45.45%) | 0 (0%) | 0 (0%) |
G3 - n (%) | 1 (8.33%) | 0 (0%) | 0 (0%) | 9 (75%) | 2 (16.66%) |
G4 - n (%) | 5 (38.46%) | 0 (0%) | 0 (0%) | 3 (23.07) | 5 (38.46%) |