The NFC-G sample preparation steps. The glass slide surface is treated by oxygen plasma (1) followed by spin coating of 5.0 wt% glycerol anchor layer (2), NFC-G spin coating (3), and PEDOT:PSS spin coating (4). The drop cast NFC-G samples were prepared by an additional step before the PEDOT:PSS spin coating