Dimension properties of electrospun PDLLA/collagen scaffolds.

Composite Scaffolds Fibre Diameter (nm) Porosity % Fibre Diameter (nm) Porosity %
As-Spun After Wet Immersion
PDL20 1686 ± 55.5 70.1 ± 2.43 N/A 0.35 ± 0.23
PDL40 1014 ± 83.4 68.5 ± 1.16 N/A 9.1 ± 2.11
PDL60 668 ± 23.4 65.4 ± 1.42 701 ± 19.9 54.9 ± 1.53
PDL80 330 ± 13.2 59.5 ± 8.71 384 ± 10.2 53.7 ± 2.76
Incubation/no GTA Incubation/GTA
PDL20 N/A 0.6 ± 0.02 1692 ± 71.6 55.36 ± 3.35
PDL40 1303 ± 48.5 59.8 ± 3.08 1052 ± 35.3 62.8 ± 3.97
PDL60 770 ± 23.3 55.7 ± 4.2 677 ± 47.4 63.3 ± 1.05
PDL80 472 ± 15.5 54.5 ± 2.89 336 ± 39.7 51.7 ± 2.05