Figure 6.
TEM images of TiO2 powder sintered at 900°C for 2 hours (insets: SAED patterns).
Abbreviations: TEM, transmission electron microscope; TiO2, titanium dioxide; SAED, selected area electron diffraction.
TEM images of TiO2 powder sintered at 900°C for 2 hours (insets: SAED patterns).