Skip to main content
. 2015 Oct 13;10(10):e0140278. doi: 10.1371/journal.pone.0140278

Fig 3. Surface contact angles of the control and plasma treatment surfaces.

Fig 3

The surface contact angles of zirconia decreased significantly after the helium APDBD plasma treatment for 30, 60 or 90 s. Data are shown as means ± SD (n = 9). Identical letters indicate no significant difference for each value (p > 0.05).