. 2015 Oct 12;10:6317–6329. doi: 10.2147/IJN.S86440

Table 3.

Lag phase and growth rate of the growth curves of survival on hydroxyapatite bone cement containing organic nanoparticles

Concentration of nanoparticles (% w/w) λ (hour) Growth rate (hour−1)
S. aureus
 0 0.11±0.02 0.15±0.02
 0.1 0.13±0.02 0.16±0.03
 0.5 2.11±0.08 0.12±0.03
 1 3.81±0.36 0.06±0.02
 5 >24 No growth
MRSA
 0 1.25±0.22 0.27±0.03
 0.1 1.44±0.26 0.31±0.05
 0.5 2.25±0.35 0.31±0.04
 1 10.02±0.73 0.26±0.07
 5 >24 No growth
A. baumannii
 0 2.29±0.36 0.22±0.01
 0.1 2.34±0.43 0.18±0.02
 0.5 1.78±0.13 0.20±0.02
 1 >24 No growth
 5 >24 No growth
S. epidermidis
 0 1.60±1.24 0.17±0.00
 0.1 1.23±0.55 0.14±0.01
 0.5 2.12±0.25 0.14±0.02
 1 8.45±1.27 2.42±5.22
 5 >24 No growth

Note: Mean ± standard deviation.

Abbreviations: MRSA, methicillin-resistant Staphylococcus aureus; S. aureus, Staphylococcus aureus; A. baumannii, Acinetobacter baumannii; S. epidermidis, Staphylococcus epidermidis.