Skip to main content
. 2015 Jun 12;4(5):595–599. doi: 10.1002/open.201500100

Figure 5.

Figure 5

The oxidation of silver nanoparticles on a glassy carbon electrode in 0.1 m NaNO3 (black) and 0.1 m NaH2PO4 (red) at a scan rate of 0.05 V s−1. Each data point consists of a minimum of three repeats.