Skip to main content
. 2015 Oct 23;5:15664. doi: 10.1038/srep15664

Figure 1. XRD patterns of (a) fresh Pd/rGO and (b) Pd/rGO after 5 reuses.

Figure 1

The diffraction peaks at 40.1°, 46.6°, 68.0°, 82.1° and 86.4° correspond to Pd (111), Pd (200), Pd (220), Pd (311) and Pd (222), respectively. The diffraction peak at 25.1° is ascribed to the 0.335 nm interlayer distance of graphite sheet in the rGO.