Skip to main content
. 2015 Oct 21;10(10):e0140374. doi: 10.1371/journal.pone.0140374

Fig 4. Scanning electron micrographs at different magnifications of: A and B) uncoated zirconia abutment, C and D) G3 glassy coated zirconia abutment, E and F) ZnO35 coated zirconia abutment, G and H) G1n-Ag coated zirconia abutment.

Fig 4