Skip to main content
. 2015 Sep;10(9):1523–1527. doi: 10.4103/1673-5374.165527

Figure 2.

Figure 2

Stress-strain curves of Tiansu silicone membrane (A) and SMI silicone membrane (B).

1, 2, 3: Results of cycles 1, 2, and 3, respectively, at a velocity of 10 mm/min. A triangle represents the end of tension, and mainly contains data before rupture.