Fig 5. Representative EDIC images of biofilm development on hydrogel latex catheter sections.

Fig 5

a. 3 days exposure showing thick microcrystalline layer. b. 9 days exposure showing development of a three-dimensional, diffuse crystalline structure, extending out from the surface. (Magnification x 1000, bar = 10 μm).