Properties of TiO2 catalyst on supports according to XRD pattern analysis using the (211) reflection peaks of anatase TiO2

Catalyst 2θ (°) FWHM (°) Crystal size (nm)
TiO2 54.43 1.91 4.69
TiO2/SBA-15 54.04 1.97 4.53
TiO2/ CNT 54.18 1.99 4.48
TiO2/SBA-CNT 54.30 1.84 5.86