Skip to main content
. 2015 Nov 3;5:16052. doi: 10.1038/srep16052

Figure 4. SEM images of untreated and treated films.

Figure 4

Low-magnification view of an untreated CdTe NW film (a) and a film that has been compressed at 400 MPa, then sintered at 20 mJ/cm2. (b) Scale bar = 50 nm.