Skip to main content
. 2015 Nov 16;5:16618. doi: 10.1038/srep16618

Figure 7.

Figure 7

(a) Enlargement of the voltage window evaluated by CD at 0.2 A g−1, (b) long-term stability at different cell voltages in the 1.1–1.7 V range evaluated by charge-discharge at a constant current of 5 A g−1 and (c) ESR resistance variation ratio (Rn/R1× 100, where Rn is the resistance at the nth cycle and R1 at the 1st cycle) at different cell voltages in the 1.1–1.7 V range evaluated by charge-discharge at a constant current of 5 A g−1 for the microporous materials in 1 M Li2SO4 electrolyte.