. 2015 May 29;5:10600. doi: 10.1038/srep10600

Figure 1.

Figure 1

(Zhang). Atom maps revealing the formation of Y-Ti-O enriched nanoclusters in the as-milled specimen (a) and the specimens annealed at 500°C for (b) 1 h, (c) 10 h, and (d) 24 h. Solute clustering occur during mechanical alloying and some large solute clusters nucleate, forming the Ti-Y-O nanoclusters (circled in Fig. 1a).