Figure 5

Decay of the logarithmic peak intensity ln[I(TS)] with increasing surface temperature TS of the first order diffraction peak along ΓM. The plot shows the decay for both Ni(111) and graphene/Ni(111), measured at an incident beam energy of 8 meV.