Skip to main content
. 2015 Sep 25;6:1939–1945. doi: 10.3762/bjnano.6.198

Figure 4.

Figure 4

Amount of PEG molecules of various molecular weights released from PCL, PVA and PLA nanofibers immersed to distilled water within 72 h at 20 °C.