Skip to main content
. 2015 Nov 27;5:17371. doi: 10.1038/srep17371

Figure 2. SEM images of the SiNWs obtained by varying the thermal oxidation time.

Figure 2

(a) 0 min; (b) 45 min; (c) 90 min; (d) 180 min; (c) 300 min; (d) 600 min.