Figure 8.

Figure 8

(a) Ex situ XRD patterns of the C-RZnHCF electrode at various discharge and charge states in the first cycle. D0 is the original one before electrochemical measurement. (b) Typical discharge/charge profiles of C-RZnHCF electrodes obtained at corresponding discharge/charge stages captured for ex situ XRD measurement. For example, after the discharge stage of D1, the electrode was characterized by XRD to get the D1 XRD pattern. (c) Changes of the value of lattice parameter (a) during Zn-ion insertion and extraction.