Skip to main content
. 2015 Oct 23;137(45):14288–14294. doi: 10.1021/jacs.5b06892

Figure 6.

Figure 6

(a) TEM (stained with 1% uranyl acetate) and (b) cryo-TEM (unstained) of TANI(CSA)2-PTAB (4 × 10–3 M). (c) Histogram showing comparison of measured nanowire widths for EB and CSA-doped TANI-PTAB. Scale bars: 50 nm.