Skip to main content
. Author manuscript; available in PMC: 2017 Jan 1.
Published in final edited form as: Dent Mater. 2015 Sep 28;32(1):43–53. doi: 10.1016/j.dental.2015.09.008

Figure 1.

Figure 1

SEM of a polymeric strut cross section (A); the resulting defect in a sintered scaffold (B) and successful defect elimination after a second coating followed by sintering (C). Bar=100 µm.