Cycling performances of ASGF, SGF, and pure SnO2 nanoparticles at specific currents of 200 mA g−1 (A) and 1000 mA g−1 (B); rate capability of ASGF and SGF at current densities from 100 mA g−1 to 3000 mA g−1 (C); CV curves of the first three cycles of ASGF at a scanning rate of 0.5 mV s−1 (D).