Figure 1.

Figure 1

Polyplex size in DMEM containing 10% FBS monitored at an initial formulation of 200 μM in water and diluted to 100 μM in DMEM containing 10% FBS (0 h), and at 1, 2, and 4 h post dilution. The numbers on the x-axis indicate the N/P of the sample. The error bars represent standard deviation of triplicate measurements. Polylexes that were very large and beyond the upper detection limit of our DLS instrument were marked with an asterisk (*).