Skip to main content
. 2016 Jan 6;3(1):49–56. doi: 10.1093/rb/rbv028

Figure 6.

Figure 6.

three-dimensional images of (a) pure Mg and (b) AZ91 alloy before the corrosion and (c) pure Mg and (d) AZ91 alloy under TEL with a thickness of 50 μm and (e) pure Mg and (f) AZ91 alloy under TEL with a thickness of 500 μm