Skip to main content
. 2016 Jan 19;6:19468. doi: 10.1038/srep19468

Figure 3. Fatigue life (average number of cycles to failure) of Sr-HT-Gahnite scaffolds under cyclic compressive stress at 60 and 70% porosity.

Figure 3

(*Significant difference between groups, p < 0.05). The numbers on top of each bar indicates the number of scaffolds that survived 106 cycles after finishing the test.