Table 1.
Sample | Mean pore diameter (μm) | Porosity (%) | Magnification 100X | Magnification 300X |
---|---|---|---|---|
Nonwoven PET | 59±47 | 85.9 | ||
Nonwoven Chitosan | 55±43 | 89.7 | ||
Chitosan nonwoven (plasma-treated) | 63±49 | 91.6 | ||
PolySTAT/Chitosan | 48±37 | 85.9 | ||
Celox® Rapid | 47±34 | 73.2 |