Published in final edited form as: Acta Biomater. 2015 Nov 28;31:178–185. doi: 10.1016/j.actbio.2015.11.017

Table 1.

Mean pore size, porosity, and SEM images of nonwoven PET, nonwoven chitosan, PolySTAT/chitosan, and Celox® Rapid.

Sample Mean pore diameter (μm) Porosity (%) Magnification 100X Magnification 300X
Nonwoven PET 59±47 85.9 graphic file with name nihms741439t1.jpg graphic file with name nihms741439t2.jpg
Nonwoven Chitosan 55±43 89.7 graphic file with name nihms741439t3.jpg graphic file with name nihms741439t4.jpg
Chitosan nonwoven (plasma-treated) 63±49 91.6 graphic file with name nihms741439t5.jpg graphic file with name nihms741439t6.jpg
PolySTAT/Chitosan 48±37 85.9 graphic file with name nihms741439t7.jpg graphic file with name nihms741439t8.jpg
Celox® Rapid 47±34 73.2 graphic file with name nihms741439t9.jpg graphic file with name nihms741439t10.jpg