Skip to main content
. 2016 Jan 15;16(1):103. doi: 10.3390/s16010103

Figure 17.

Figure 17

Changes of the resistance of the structure with graphite oxide (dosed atmosphere: nitrogen dioxide with concentration of 125 ppm, 25 ppm, 5 ppm and 500 ppm, temperature of the sample: 100 °C)