Skip to main content
. 2016 Jan 1;23(Pt 1):260–266. doi: 10.1107/S1600577515018007

Figure 8.

Figure 8

Consecutive ‘up’ and ‘down’ XANES spectra of a Cu metal foil at the Cu K-edge measured at different oscillation frequencies.