Figure 5.

Figure 5

Calibration curves in terms of the percentage relative electrical resistance change for a chemiresistor based on pristine and Au@ZnO annealed at A) 300 °C and B) 550 °C, towards NO2 gases, at a working temperature of 300 °C.