FIGURE 8

Antibiofouling activity of EPS273 in marine environment. (A) and (B) are images of biofouling formation on glass slides precoated by paints with or without EPS273 after 1 or 2 weeks in the ocean environment, respectively. (C) and (D) are the relative amounts of bacteria and diatoms from corresponding glass slides, respectively. The amount of bacteria or diatoms from glass slides without EPS273 was set at 100%. Error bars indicate the standard deviations of three measurements. P < 0.05 versus the control.