Table 2.
Exact dimensions, breaking force, and bending strength of the Er,Cr:YSGG irradiated specimens (group 2). The mean value of the bending strength is 96.08 MPa with a standard deviation of 28.08 MPa.
| Number | Thickness/mm | Width/mm | Breaking force/N | Bending strength/MPa |
|---|---|---|---|---|
| 1 | 1.49 | 1.90 | 35.70 | 68.55 |
| 2 | 1.65 | 1.80 | 59.80 | 98.84 |
| 3 | 1.54 | 1.87 | 67.70 | 123.65 |
| 4 | 1.83 | 1.46 | 89.10 | 147.61 |
| 5 | 1.16 | 1.88 | 21.20 | 67.88 |
| 6 | 1.64 | 1.95 | 72.10 | 111.35 |
| 7 | 1.27 | 1.75 | 37.30 | 107.04 |
| 8 | 1.38 | 1.89 | 33.10 | 74.49 |
| 9 | 1.50 | 1.83 | 61.20 | 120.39 |
| 10 | 1.20 | 1.80 | 18.00 | 56.25 |
| 11 | 1.44 | 1.74 | 27.40 | 61.51 |
| 12 | 0.93 | 1.70 | 20.30 | 111.83 |
| 13 | 1.07 | 1.86 | 27.90 | 106.12 |
| 14 | 1.14 | 1.87 | 21.20 | 70.66 |
| 15 | 1.68 | 1.88 | 79.30 | 121.05 |
| 16 | 1.55 | 1.73 | 76.50 | 149.09 |
| 17 | 1.14 | 1.90 | 24.90 | 81.68 |
| 18 | 1.13 | 2.37 | 25.50 | 68.25 |
| 19 | 1.98 | 1.00 | 53.70 | 110.95 |
| 20 | 1.65 | 1.80 | 48.20 | 79.67 |