. 2015 Dec 30;24(4):265–274. doi: 10.5978/islsm.15-OR-16

Fig. 3:

Fig. 3:

Filtek™ supreme XTE flow polymerization depth test. The laser device produced worse performances at each energy level; moreover, no significant differences were observed between the groups that were polymerized with the laser, including between the 4 Joule and 32 Joule groups (DL, diode LED Valo; HL, halogen lamp; L, 405 nm laser).