Figure 3. The characterization of the PMO nanocubes with different sizes.

Figure 3

Small-angle XRD patterns (A), nitrogen adsorption–desorption isotherms (B) and the corresponding NLDFT pore size distributions (inset B) of the extracted ethane-bridged PMO materials with different particle sizes of 150 nm (black), 200 nm (red), 400 nm (green) and 600 nm (blue).