Table 2. The mean surface microhardness values in groups 4-6 treated with fluoride varnish, casein phosphopeptide-amorphous calcium phosphate complex, and Remin Pro® .

Groups Primary microhardness Microhardness after 4 days demineralization Microhardness after 1 month treatment Microhardness after re-demineralization
M * SD ** M SD M SD M SD
Group 1 (fluoride varnish) 7.339 5.60 6.223 5.39 7.273 3.25 3.267 02.39
Group 2 (CPP-ACP) 6.331 05.31 3.235 5.27 9.411 9.35 2.334 09.38
Group 3 (Remin Pro) 8.337 02.69 8.230 1.45 5.333 2.25 2.289 1.37