Skip to main content
. Author manuscript; available in PMC: 2017 Mar 1.
Published in final edited form as: Biomaterials. 2016 Jan 7;83:332–346. doi: 10.1016/j.biomaterials.2016.01.020

Figure 2.

Figure 2

Cumulative PLL-FITC release from (A) 10K OPF hydrogels and (B) 35K OPF hydrogels loaded with PLL at 500 ng/hydrogel, 5 µg/hydrogel, or 20 µg/hydrogel over 28 days is shown. Visualization of uniformly distributed PLL-FITC loaded into hydrogel constructs at each concentration, which is shown at days 7 and 28 after incorporation for (C) 10K hydrogels and (D) 35K hydrogels. Scale bar = 200 µm.