Skip to main content
. Author manuscript; available in PMC: 2016 Dec 2.
Published in final edited form as: RSC Adv. 2015 Dec 2;5(128):105636–105642. doi: 10.1039/C5RA24097B

Table 1.

Summary of measured deviations of mean phase lag and strain amplitude of fixed cells and property changes (ω = 20 Hz).

Chemical
modification
δ ε0 E η

Measured variable Property changes due to
fixation
Unmodified 0.284 ± 0.097 π 2.80 % ± 1.09 % - -
Glutaraldehyde (0.0025% v/v) 0.208 ± 0.096 π 2.24 % ± 0.90 % Increase Increase
Diamide (3.8mM) 0.241 ± 0.113 π 3.08 % ± 1.25 % Increase Constant
Swelling (150 mOsm) 0.239 ± 0.097 π 2.47 % ± 1.00 % Increase Constant