Table 1. Layer model and fitting parameters for the Au film containing a monolayer of R6G molecules.
layer | Au film | R6G/Au film | △ | ||||||||
---|---|---|---|---|---|---|---|---|---|---|---|
d | ε′ | ε″ | d | ε′ | ε″ | ∆ d | ∆ ε′ | ∆ε″ | |||
1 | Prism | ∞ | 3.4 | 0 | Prism | ∞ | 3.4 | 0 | 0 | 0 | 0 |
2 | Cr | 2.1 | −4.4 | 18.1 | Cr | 2.1 | − 4.4 | 18.1 | 0 | 0 | 0 |
3 | Gold | 50.0 | −11.5 | 1.4 | Gold | 50.0 | −11.5 | 1.4 | 0 | 0 | 0 |
4 | Air | ∞ | 1 | 0 | R6G | 0.6 | 4.4 | 5.9 | – | – | – |
5 | Air | ∞ | 1 | 0 | – | – | – |
Comparison of the changes in the dielectric constant as a function of the monolayer of R6G molecules on Au.