. 2015 Oct 19;27(45):7356–7364. doi: 10.1002/adma.201502437

Figure 5.

Figure 5

a) Transfer and b) output characteristics of aligned FET with μ sat = 6.7 cm2 V−1 s−1. c) Hole mobilities of FETs with aligned polymer layers (room temperature), parallel and perpendicular to shearing direction. Error bars represent the standard deviation over multiple samples. d) Temperature dependence of mobilities for spin‐coated and aligned FETs. Arrhenius fits are labeled with the respective extracted activation energies.