Skip to main content
. Author manuscript; available in PMC: 2016 Sep 1.
Published in final edited form as: Dent Mater. 2015 Jul 10;31(9):1109–1118. doi: 10.1016/j.dental.2015.06.011

Figure 7.

Figure 7

Scanning electron micrographs showing details of the fracture surfaces resulting from fatigue crack growth of the bonded interface specimens. Above shows failure within the hybrid layers of a) SB at 2000X, b) SB at 8000X, c) SBMP at 2000X, d) SBMP at 8000X. The arrows in each figure represent the direction of cyclic crack extension.