Skip to main content
. Author manuscript; available in PMC: 2016 Mar 15.
Published in final edited form as: RSC Adv. 2015 Feb 17;5(27):21301–21309. doi: 10.1039/C5RA00508F

Fig. 4.

Fig. 4

SEM micrographs of 3-D porous scaffolds prepared by phase separation using: (A) 3 wt%, (B) 5 wt%, and (C) 9 wt% of PPF-co-PLLA in a dioxane/water (85/15 wt/wt) solution followed by quenching at 20 °C for 1 min, freezing at −80 °C for 2 hours and lyophilization for 3 days.