Fig. 7.

Fig. 7

SEM micrographs of 3-D porous scaffolds prepared by phase separation of 7% PPF-co-PLLA in dioxane/water (85/15, wt/wt) solution with freezing temperature of (A) −20 °C, (B) −80 °C, and (C) −196 °C.