Fig 7. Example of failure modes through examination of the bonded surfaces after lap shear test completion.

Fig 7

Left: cohesive (250 mg rosin/250 mg beeswax/50 mg ochre), the adhesive remains evenly bonded to both sides; middle: mixed-mode (400 mg rosin/100 mg beeswax/100 mg ochre), the adhesive favours one side, but remains bonded to both some areas; right: adhesive failure (400 mg rosin/100 mg beeswax/50 mg ochre), the adhesive remains bonded to one side only.