Skip to main content
. Author manuscript; available in PMC: 2017 Apr 1.
Published in final edited form as: J Mech Behav Biomed Mater. 2015 Dec 12;57:128–138. doi: 10.1016/j.jmbbm.2015.12.001

Fig. 6.

Fig. 6

Pre-strain reduction in wet vs. dry bone in tension (A) and in compression (B): Pre-strain reduction index (ζ) varies from one to zero, one indicating the original pre-strained state of the mineral phase and zero indicating a complete removal of pre-strain. Dry specimens exhibited no reduction in pre-strain, whereas wet specimens showed significant reduction in pre-strain. In compression, the pre-strain reduction index saturated at bulk strains higher than 2%.