Skip to main content
. 2016 Apr 1;6:23627. doi: 10.1038/srep23627

Figure 5.

Figure 5

Illustration of the corrosion mechanism for Pt discs patterned pure iron: (a) initial corrosion reaction; (b) and (c) were the formation procedure of hydroxide layer; (d) after Pt discs fell off, the degradation rate of pure iron can be continuing accelerated by the corrosion pits.