Skip to main content
. 2016 Apr 13;6:24189. doi: 10.1038/srep24189

Figure 5.

Figure 5

Shell to core ratio for different annealing times of polycrystalline and single-crystal NWs, showing that after 24 hours, the polycrystalline NWs are fully oxidized, while the maximum shell thickness for single-crystal NWs is 12 nm, even after 72 hours.