Skip to main content
. 2016 Apr 19;11(4):e0153685. doi: 10.1371/journal.pone.0153685

Table 3. Results of physical characteristics including average yield weight, microencapsulation yield, average size, and loading efficiency for astaxanthin encapsulated beads prepared with various formulations.

Code name Average Yield Weight (g) Microencapsulation Yield (%) Average Size (μm) Loading Efficiency (%)
1A0.5T2C 0.29±0.03 63.8±3.6 690.5±74.5 96.6±3.6
1A0.5T10C 0.37±0.06 29.2±4.5 754.2±80.7 95.0±2.9
1A2T2C 0.29±0.02 63.4±2.4 692.7±58.8 86.2±4.2
1A2T10C 0.33±0.04 25.8±4.9 685.9±55.1 82.5±4.2
2A0.5T2C 0.46±0.04 79.0±4.6 825.4±52.5 86.0±3.2
2A0.5T10C 0.58±0.08 41.1±7.3 906.4±35.6 97.3±3.8
2A2T2C 0.46±0.04 80.3±3.8 842.7±45.0 82.0±1.8
2A2T10C 0.62±0.08 44.2±8.2 883.6±62.2 93.3±2.0
3A0.5T2C 0.64±0.02 91.3±2.6 939.4±47.9 86.8±2.9
3A0.5T10C 0.85±0.05 55.7±6.1 964.0±43.0 89.6±2.5
3A2T2C 0.69±0.02 97.9±2.8 1011.8±50.4 99.2±1.7
3A2T10C 0.97±0.03 63.2±3.0 1044.4±64.6 100.0±4.2